DESCRIPTION OF KF-D
Light gray powder with specific smell. After application, the smell disappears.
This inorganic compound works as an admixture to the cement containing Earth-Materials-Sealants (EMS).

BENEFITS

USES OF KF-D

APPLICATION 
Add 5.5 Lbs of KF-D per 200 Lbs of cement or 2.5 Kg of KF-D per 100 Kg of cement to EMS and mix for 10 min.
Add pure water to produce a water to cement ratio of 0.38.
Mix for 5 minutes and unload into the hopper of pump station.
Apply mix through injectors into the targeted damaged areas.

The KF-D and EMS premix can be poured onto soils with or without subsequently mixing with the soil for stabilization and waterproofing of soaked areas.    

COMPACTION OF TREATED SPECIMENS

Specimens             Untreatd, %     Treated, %                                                          
Brown Clay Sand        86                      97
Gravelly Clay                88                      95
Gravel & Sand             79                      96
Masonry                       66                      89
Light Concrete            69                      98
              TECHNICAL DATA OF KF-D PREMIXED WITH EMS

_Final hardening is adjustable from______10 to 40 minutes.

_Minimum temperature on site is_______- 15C or 5F

_Slump____________________________2.5 cm or 1"

_Shinkage__________________________300 micro strain

_Compressive Strength after 3 days         21 MPa/3000 PSI 
                                             7 days ____30 MPa/4260 PSI

_Reduction of hydraulic conductivity_____80%